Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Composition
1 micrograph for composition Low concentration (<0.3 vol%) suspension in water, ordered by micrograph number.
![]() |
Micrograph
563
:
Carbon nanotubes System: Carbon nanotube, Composition: Low concentration (<0.3 vol%) suspension in water Field emission gun scanning electron microscopy (FEGSEM) 99 nm |