Composition
3 micrographs for composition Bi 50, Sn 50 (wt%), ordered by micrograph number.
![]() |
Micrograph
756
:
Bi 50, Sn 50 (wt%) System: Bi-Sn, Composition: Bi 50, Sn 50 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 300 μm |
![]() |
Micrograph
757
:
Bi 50, Sn 50 (wt%) System: Bi-Sn, Composition: Bi 50, Sn 50 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 100 μm |
![]() |
Micrograph
758
:
Bi 50, Sn 50 (wt%) System: Bi-Sn, Composition: Bi 50, Sn 50 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 10 μm |