DoITPoMS

Composition

11 micrographs for composition Not specified (System: Al), ordered by micrograph number.

Showing 1 - 10 of 11 micrographs Page 1 2 | Previous | Next

Link to full record for micrograph 82 Micrograph 82 : Aluminium, fracture surface
System: Al, Composition: Not specified
Scanning electron microscopy (SEM)
15 μm
Link to full record for micrograph 83 Micrograph 83 : Aluminium, fracture surface
System: Al, Composition: Not specified
Scanning electron microscopy (SEM)
50 μm
Link to full record for micrograph 629 Micrograph 629 : FORMGRIP closed cell aluminium foam
System: Al, Composition: Not specified
Photography (no microscope)
6 mm
Link to full record for micrograph 630 Micrograph 630 : FOAMCARP closed cell aluminium foam
System: Al, Composition: Not specified
Photography (no microscope)
6 mm
Link to full record for micrograph 631 Micrograph 631 : Coarse open celled aluminium foam produced by infiltration of sintered salt (FOAM-U-LIKE)
System: Al, Composition: Not specified
Photography (no microscope)
6 mm
Link to full record for micrograph 632 Micrograph 632 : Open-celled aluminium foam
System: Al, Composition: Not specified
Photography (no microscope)
8 mm
Link to full record for micrograph 633 Micrograph 633 : Cross-section of an aluminium foam slab produced by gas injection
System: Al, Composition: Not specified
Photography (no microscope)
10 mm
Link to full record for micrograph 634 Micrograph 634 : Solid-gas eutectic solidification (Gasar) aluminium foam
System: Al, Composition: Not specified
Photography (no microscope)
120 μm
Link to full record for micrograph 635 Micrograph 635 : Open celled aluminium foam produced by infiltration of sintered salt
System: Al, Composition: Not specified
Scanning electron microscopy (SEM)
400 μm
Link to full record for micrograph 636 Micrograph 636 : Alporas' closed cell aluminium foam
System: Al, Composition: Not specified
Photography (no microscope)
6 mm

Showing 1 - 10 of 11 micrographs Page 1 2 | Previous | Next

List all compositions