Composition
2 micrographs for composition Mostly clay (which consists of alumina and silica), ordered by micrograph number.
![]() |
Micrograph
187
:
Part of a Denby pottery mug, showing the glaze on the surface System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica) Reflected light microscopy 200 μm |
![]() |
Micrograph
188
:
Part of a Denby pottery mug System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica) Reflected light microscopy 200 μm |