Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Contributor
44 micrographs contributed by Dr K M Knowles, ordered by micrograph number.
| Showing 21 - 30 of 44 micrographs | Page 1 2 3 4 5 | Previous | Next |
![]() |
Micrograph
180
:
Oven-to-tableware showing the glaze on the surface, using a sensitive tint plate System: Miscellaneous, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 200 μm |
![]() |
Micrograph
181
:
Oven-to-tableware System: Miscellaneous, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
182
:
Oven-to-tableware System: Miscellaneous, Composition: Not specified Transmitted polarised light microscopy 100 μm |
![]() |
Micrograph
183
:
Oven-to-tableware System: Miscellaneous, Composition: Not specified Transmitted polarised light microscopy 250 μm |
![]() |
Micrograph
184
:
Oven-to-tableware System: Miscellaneous, Composition: Not specified Transmitted polarised light microscopy 250 μm |
![]() |
Micrograph
185
:
Silicon Nitride-bonded Silicon Carbide System: Silicon nitride-bonded silicon carbide, Composition: Particles of SiC in a reaction-bonded Si3N4 matrix Reflected light microscopy 250 μm |
![]() |
Micrograph
186
:
Silicon Carbide from within a Silicon Nitride-bonded Silicon Carbide sample System: Silicon nitride-bonded silicon carbide, Composition: Particles of SiC in a reaction-bonded Si3N4 matrix Reflected light microscopy 25 μm |
![]() |
Micrograph
187
:
Part of a Denby pottery mug, showing the glaze on the surface System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica) Reflected light microscopy 200 μm |
![]() |
Micrograph
188
:
Part of a Denby pottery mug System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica) Reflected light microscopy 200 μm |
![]() |
Micrograph
542
:
Devitrified Glass: glass sample heated at 900°C for 17 hours. System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
| Showing 21 - 30 of 44 micrographs | Page 1 2 3 4 5 | Previous | Next |