Contributor
4 micrographs contributed by Dr V Gergely, ordered by micrograph number.
![]() |
Micrograph
629
:
FORMGRIP closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |
![]() |
Micrograph
633
:
Cross-section of an aluminium foam slab produced by gas injection System: Al, Composition: Not specified Photography (no microscope) 10 mm |
![]() |
Micrograph
634
:
Solid-gas eutectic solidification (Gasar) aluminium foam System: Al, Composition: Not specified Photography (no microscope) 120 μm |
![]() |
Micrograph
636
:
Alporas' closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |