Full Record for Micrograph 285
[107 KB]
View micrograph
.. in new window
View micrograph and record
.. in new window
You can also view and download the micrographs on Flickr
- Micrograph no
- 285
- Brief description
- Chromitised low carbon steel
- Keywords
- alloy
, carbon, carburisation
, iron, metal, steel 
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C low (wt%)
- Standard codes
- Reaction
- Processing
- chromitised
- Applications
- Sample preparation
- Nital
- Technique
- Reflected light microscopy
- Length bar
- 800 μm
- Further information
- Low carbon steel that has had additional chromium added. Chromium increases response to heat treatment and increases depth of hardness penetration.
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds