- Micrograph no
- 335
- Brief description
- Medium carbon steel, slow quenched
- Keywords
- alloy
, carbon, iron, metal, steel
, Widmanstätten 
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C 0.3 (wt%)
- Standard codes
- Reaction
- Processing
- Slow quenched 950 ºC
- Applications
- Sample preparation
- Nital
- Technique
- Reflected light microscopy
- Length bar
- 100 μm
- Further information
- Medium carbon steel that has been slow quenched, and resulting in the production of Widmanstätten ferrite.
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02