Full Record for Micrograph 644
[57 KB]
View micrograph
.. in new window
View micrograph and record
.. in new window
You can also view and download the micrographs on Flickr
- Micrograph no
- 644
- Brief description
- Carbon nanotubes, coated with a conducting polymer
- Keywords
- carbon, carbon nanotube, coating, conducting polymer, nanotube
, polymer
, polypyrrole - Categories
- Polymer
- System
- Carbon nanotube
- Composition
- Coating of polypyrrole
- Standard codes
- Reaction
- Processing
- The composite films were formed by electrochemically polymerising a conducting polymer, polypyrrole, onto unaligned carbon nanotubes.
- Applications
- These fine conducting composites have many potential applications in microelectronic devices and sensors.
- Sample preparation
- Technique
- Scanning electron microscopy (SEM)
- Length bar
- 100 nm
- Further information
- Carbon nanotubes are a long, tubular form of carbon that has an extremely high surface area. Conducting polymers, as their name suggests, are a group of polymers that exhibit excellent electrical conductivity, in some cases reaching that of copper.
- Contributor
- M Hughes
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 03/10/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs