58 micrographs for keyword composite material, ordered by micrograph number.


Showing 1 - 10 of 58 micrographs Page 1 2 3 4 5 6 | Previous | Next

Link to full record for micrograph 129 Micrograph 129 : Woven E - glass fibres in a DERAKANE (TM) matrix
System: Glass fibre composite, Composition: Not specified
Reflected light microscopy
800 μm
Link to full record for micrograph 130 Micrograph 130 : Woven E - glass fibres in a DERAKANE (TM) matrix
System: Glass fibre composite, Composition: Not specified
Reflected light microscopy
200 μm
Link to full record for micrograph 131 Micrograph 131 : Unidirectional T800 carbon fibres in an MTM49 epoxy matrix.
System: CCcomposite, Composition: Not specified
Reflected light microscopy
250 μm
Link to full record for micrograph 132 Micrograph 132 : Woven T800 carbon fibres in an MTM49 epoxy matrix.
System: CCcomposite, Composition: Not specified
Reflected light microscopy
200 μm
Link to full record for micrograph 151 Micrograph 151 : Alumina-graphite brick
System: Al2O3-C-Si, Composition: Al2O3, C up to 30 (wt%), Si few%
Reflected light microscopy
400 μm
Link to full record for micrograph 166 Micrograph 166 : Carbon-carbon composite
System: CCcomposite, Composition: Not specified
Reflected light microscopy
250 μm
Link to full record for micrograph 167 Micrograph 167 : Carbon-carbon composite
System: CCcomposite, Composition: Not specified
Reflected light microscopy
100 μm
Link to full record for micrograph 168 Micrograph 168 : Carbon-carbon composite
System: CCcomposite, Composition: Not specified
Reflected light microscopy
250 μm
Link to full record for micrograph 169 Micrograph 169 : Carbon-carbon composite
System: CCcomposite, Composition: Not specified
Reflected light microscopy
40 μm
Link to full record for micrograph 193 Micrograph 193 : MgO-C Refractory Brick
System: MgO-C, Composition: MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition
Reflected light microscopy
200 μm