Full Record for Micrograph 129
[220 KB]
View micrograph
.. in new window
View micrograph and record
.. in new window
You can also view and download the micrographs on Flickr
- Micrograph no
- 129
- Brief description
- Woven E - glass fibres in a DERAKANE (TM) matrix
- Keywords
- composite material
, glass fibres 
- Categories
- Composite
- System
- Glass fibre composite
- Composition
- Not specified
- Standard codes
- Reaction
- Processing
- Manufactured by a vacuum assisted resin infusion process and cured at room temperature.
- Applications
- Sample preparation
- Ground and Polished
- Technique
- Reflected light microscopy
- Length bar
- 800 μm
- Further information
- Contributor
- S Clifford
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 09/01/02