4 micrographs for system Glass fibre composite, ordered by micrograph number.
![]() |
Micrograph
129
:
Woven E - glass fibres in a DERAKANE (TM) matrix System: Glass fibre composite, Composition: Not specified Reflected light microscopy 800 μm |
![]() |
Micrograph
130
:
Woven E - glass fibres in a DERAKANE (TM) matrix System: Glass fibre composite, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
626
:
Glass fibre reinforced thermoplastic matrix composite System: Glass fibre composite, Composition: Polypropylene matrix with glass fibre Scanning electron microscopy (SEM) 60 μm |
![]() |
Micrograph
627
:
Glass fibre reinforced thermoplastic matrix composite System: Glass fibre composite, Composition: Polypropylene matrix with glass fibre Scanning electron microscopy (SEM) 200 μm |