Link to full record for micrograph 133 Micrograph 133 : Steel, austenitised at 1200 centigrade for 120 s and then transformed isothermally at 350 centigrade for 2000 s before cooling to room temperature.
System: Fe-C-X, Composition: Fe, C 0.24, Si 2.18, Mn 2.32, Ni 1.05 (wt%)
Atomic force microscopy (AFM)
1 μm
Link to full record for micrograph 134 Micrograph 134 : High carbon steel
System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%)
Transmission electron microscopy (TEM)
600 nm
Link to full record for micrograph 135 Micrograph 135 : High carbon steel
System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%)
Transmission electron microscopy (TEM)
1.5 μm
Link to full record for micrograph 311 Micrograph 311 : Fe, C 0.4 (wt%) steel, slow quenched
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 312 Micrograph 312 : Fe, C 0.4 (wt%) steel, slow quenched
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 739 Micrograph 739 : TRIP steel annealed at 775°C for 5 mins and then hold at 400°C for 150s for austenite stabilization
System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%)
Reflected light microscopy
6 μm
Link to full record for micrograph 740 Micrograph 740 : TRIP steel annealed at 775°C for 5 mins and then hold at 400°C for 40s for austenite stabilization
System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%)
Reflected light microscopy
20 μm