Keyword
29 micrographs for keyword normalising, ordered by micrograph number.
Showing 11 - 20 of 29 micrographs | Page 1 2 3 | Previous | Next |
Micrograph
248
:
Fe, C 1.3 (wt%) steel, annealed at 1000°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
249
:
Fe, C 1.3 (wt%) steel, annealed at 1000°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
250
:
Fe, C 1.3 (wt%) steel, annealed at 1000°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
253
:
Fe, C 1 (wt%) steel, normalised hypereutectoid System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
254
:
Fe, C 1 (wt%) steel, normalised hypereutectoid System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
255
:
Fe, C 1.1 (wt%) steel, normalised hypereutectoid System: Fe-C-X, Composition: Fe, C 1.1 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
256
:
Fe, C 1.1 (wt%) steel, normalised hypereutectoid System: Fe-C-X, Composition: Fe, C 1.1 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
265
:
Fe, C 0.8 (wt%) steel, eutectoid transformation, spheroidised System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
266
:
Fe, C 0.8 (wt%) steel, eutectoid transformation, spheroidised System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
267
:
Fe, C 0.8 (wt%) steel, eutectoid transformation, spheroidised System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 200 μm |
Showing 11 - 20 of 29 micrographs | Page 1 2 3 | Previous | Next |