Full Record for Micrograph 267
[233 KB]
View micrograph
.. in new window
View micrograph and record
.. in new window
You can also view and download the micrographs on Flickr
- Micrograph no
- 267
- Brief description
- Fe, C 0.8 (wt%) steel, eutectoid transformation, spheroidised
- Keywords
- alloy
, carbon, iron, metal, normalising
, spheroidised, steel 
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C 0.8 (wt%)
- Standard codes
- Reaction
- Processing
- Spheroidised
- Applications
- Sample preparation
- Nital
- Technique
- Reflected light microscopy
- Length bar
- 200 μm
- Further information
- This steel is of the eutectoid composition. Once the temperature is lowered below the eutectoid temperature, the austenite phase tends to undergo a eutectoid transformation (g to a + Fe3C). The resultant microstructure, known as pearlite, comprises alternate lamellae of cementite and ferrite. Subsequent to casting, the alloy was normalised (annealed) just below the eutectoid temperature, in order to induce the carbides to take a spherical appearance, which results in the steel becoming softer and more ductile. This is known as spheroidisation. The changes to the morphology of the cementite, compared with the normal plate-like appearance in freshly-formed pearlite, are clearly visible in this micrograph.
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02