Keyword
3 micrographs for keyword spheroidised, ordered by micrograph number.
![]() |
Micrograph
265
:
Fe, C 0.8 (wt%) steel, eutectoid transformation, spheroidised System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
266
:
Fe, C 0.8 (wt%) steel, eutectoid transformation, spheroidised System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
267
:
Fe, C 0.8 (wt%) steel, eutectoid transformation, spheroidised System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 200 μm |