17 micrographs for keyword fibre, ordered by micrograph number.


Showing 1 - 10 of 17 micrographs Page 1 2 | Previous | Next

Link to full record for micrograph 545 Micrograph 545 : Fibre reinforced magnesium aluminosilicate ceramic showing black areas of porosity
System: SiC fibre-reinforced magnesium aluminosilicate, Composition: Not specified
Reflected light microscopy
100 μm
Link to full record for micrograph 548 Micrograph 548 : Fractograph showing extensive matrix cracking and fibres bridging an opened matrix in a fibre reinforced magnesium aluminosilicate ceramic
System: SiC fibre-reinforced magnesium aluminosilicate, Composition: Not specified
Scanning electron microscopy (SEM)
200 μm
Link to full record for micrograph 550 Micrograph 550 : Micrograph showing the complex chemical reactions which arise at fibre-matrix interfaces in a fibre reinforced magnesium aluminosilicate ceramic subjected to oxidation
System: SiC fibre-reinforced magnesium aluminosilicate, Composition: Not specified
Bright-field TEM
300 nm
Link to full record for micrograph 594 Micrograph 594 : Carbon string
System: C, Composition: Not specified
Scanning electron microscopy (SEM)
400 μm
Link to full record for micrograph 596 Micrograph 596 : Glass-fibre reinforced polymer
System: Polypropylene (PP), Composition: Polypropylene with 15% glass fibres
Reflected light microscopy
400 μm
Link to full record for micrograph 597 Micrograph 597 : Frozen stress photoelastic fringe pattern during fibre pushout
System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre'
Cross-polarised light microscopy
6 mm
Link to full record for micrograph 602 Micrograph 602 : Section of a metal matrix composite (MMC)
System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (10 vol%)
Reflected light microscopy, polarised
80 μm
Link to full record for micrograph 603 Micrograph 603 : Section of a metal matrix composite (MMC)
System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (5 vol%)
Reflected light microscopy, polarised
80 μm
Link to full record for micrograph 607 Micrograph 607 : Fibre fracture in a metal matrix composite
System: Al, Composition: Commercial purity (99.5%)
Scanning electron microscopy (SEM)
4 μm
Link to full record for micrograph 618 Micrograph 618 : Fracture surface of a carbon fibre composite
System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm