17 micrographs for keyword fibre, ordered by micrograph number.
| Showing 1 - 10 of 17 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
545
:
Fibre reinforced magnesium aluminosilicate ceramic showing black areas of porosity System: SiC fibre-reinforced magnesium aluminosilicate, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
548
:
Fractograph showing extensive matrix cracking and fibres bridging an opened matrix in a fibre reinforced magnesium aluminosilicate ceramic System: SiC fibre-reinforced magnesium aluminosilicate, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
550
:
Micrograph showing the complex chemical reactions which arise at fibre-matrix interfaces in a fibre reinforced magnesium aluminosilicate ceramic subjected to oxidation System: SiC fibre-reinforced magnesium aluminosilicate, Composition: Not specified Bright-field TEM 300 nm |
![]() |
Micrograph
594
:
Carbon string System: C, Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
![]() |
Micrograph
596
:
Glass-fibre reinforced polymer System: Polypropylene (PP), Composition: Polypropylene with 15% glass fibres Reflected light microscopy 400 μm |
![]() |
Micrograph
597
:
Frozen stress photoelastic fringe pattern during fibre pushout System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre' Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
602
:
Section of a metal matrix composite (MMC) System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (10 vol%) Reflected light microscopy, polarised 80 μm |
![]() |
Micrograph
603
:
Section of a metal matrix composite (MMC) System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (5 vol%) Reflected light microscopy, polarised 80 μm |
![]() |
Micrograph
607
:
Fibre fracture in a metal matrix composite System: Al, Composition: Commercial purity (99.5%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
618
:
Fracture surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 600 μm |