Link to full record for micrograph 555 Micrograph 555 : Banded spherulites in a blend of polyethtylenes
System: Polyethylene (PE), Composition: LPE:BPE 1:3
Transmission electron microscopy (TEM)
200 nm
Link to full record for micrograph 556 Micrograph 556 : Sheaf-like arrangement of lamellae in a blend of polyethylenes
System: Polyethylene (PE), Composition: LPE:BPE 3:1
Transmission electron microscopy (TEM)
200 nm
Link to full record for micrograph 558 Micrograph 558 : High Impact Polystyrene (HIPS)
System: High Impact Polystyrene (HIPS), Composition: PS - 35%PB
Transmitted light microscopy
20 μm
Link to full record for micrograph 561 Micrograph 561 : Ordered film of carbon nanotubes
System: Carbon nanotube, Composition: Not specified
Field emission gun scanning electron microscopy (FEGSEM)
400 nm
Link to full record for micrograph 564 Micrograph 564 : Aligned array of nanotubes
System: Carbon nanotube, Composition: Not specified
Scanning electron microscopy (SEM)
25 μm
Link to full record for micrograph 566 Micrograph 566 : Inversion wall revealed by spontaneous band texture in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1)
Cross-polarised light microscopy
50 μm
Link to full record for micrograph 567 Micrograph 567 : Wedge disclinations revealed by spontaneous band texture in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1)
Cross-polarised light microscopy
50 μm
Link to full record for micrograph 568 Micrograph 568 : Strain induced birefringence in a thermoformed PET cup
System: Polyethylene terephthalate (PET), Composition: Not specified
Cross-polarised light microscopy
8 mm
Link to full record for micrograph 569 Micrograph 569 : Injection-moulded polystyrene ruler
System: Polystyrene (PS), Composition: Not specified
Cross-polarised light microscopy
11 mm
Link to full record for micrograph 572 Micrograph 572 : Birefringence in a film of polypropylene
System: Polypropylene (PP), Composition: Not specified
Cross-polarised light microscopy
10 mm