568
:
Strain induced birefringence in a thermoformed PET cup System: Polyethylene terephthalate (PET), Composition: Not specified Cross-polarised light microscopy 8 mm |
![]() |
Micrograph
569
:
Injection-moulded polystyrene ruler System: Polystyrene (PS), Composition: Not specified Cross-polarised light microscopy 11 mm |
![]() |
Micrograph
570
:
Strain-induced birefringence in a notched polycarbonate bar System: Polycarbonate (PC), Composition: Not specified Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
571
:
Strain-induced birefringence in a polycarbonate bar System: Polycarbonate (PC), Composition: Not specified Cross-polarised light microscopy 14 mm |
![]() |
Micrograph
572
:
Birefringence in a film of polypropylene System: Polypropylene (PP), Composition: Not specified Cross-polarised light microscopy 10 mm |
![]() |
Micrograph
573
:
Birefringence in a film of polyethylene System: Low density polyethylene (LDPE), Composition: Not specified Cross-polarised light microscopy 14 mm |
![]() |
Micrograph
574
:
Injection-moulded polystyrene (PS) case System: Polystyrene (PS), Composition: Not specified Cross-polarised light microscopy 14 mm |
![]() |
Micrograph
575
:
Injection-moulded protractor System: Polystyrene (PS), Composition: Not specified Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
576
:
Injection-moulded protractor System: Polystyrene (PS), Composition: Not specified Cross-polarised light microscopy 30 mm |
![]() |
Micrograph
577
:
Injection-moulded polypropylene (PP) hinge System: Polypropylene (PP), Composition: Not specified Cross-polarised light microscopy 1.4 mm |