Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
77 micrographs for keyword ceramic, ordered by micrograph number.
| Showing 51 - 60 of 77 micrographs | Page 1 2 3 4 5 6 7 8 | Previous | Next |
![]() |
Micrograph
545
:
Fibre reinforced magnesium aluminosilicate ceramic showing black areas of porosity System: SiC fibre-reinforced magnesium aluminosilicate, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
546
:
Delamination cracks seen in h-BN particles subjected to compressive stress in the (0001) planes (within a silicon nitride particulate-reinforced silicon carbide composite) System: Si3N4-SiC composite, Composition: Not specified High resolution electron microscopy (HREM) 10 nm |
![]() |
Micrograph
547
:
h-BN inclusion (precipitate) in a b-Si3N4 grain (within a silicon nitride particulate-reinforced silicon carbide composite) System: Si3N4-SiC composite, Composition: Not specified High resolution electron microscopy (HREM) 20 nm |
![]() |
Micrograph
548
:
Fractograph showing extensive matrix cracking and fibres bridging an opened matrix in a fibre reinforced magnesium aluminosilicate ceramic System: SiC fibre-reinforced magnesium aluminosilicate, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
549
:
Misoriented interphase boundary between h-BN (precipitate) and SiC grains (within a silicon nitride particulate-reinforced silicon carbide composite) System: Si3N4-SiC composite, Composition: Not specified High resolution electron microscopy (HREM) 1.2 nm |
![]() |
Micrograph
550
:
Micrograph showing the complex chemical reactions which arise at fibre-matrix interfaces in a fibre reinforced magnesium aluminosilicate ceramic subjected to oxidation System: SiC fibre-reinforced magnesium aluminosilicate, Composition: Not specified Bright-field TEM 300 nm |
![]() |
Micrograph
551
:
A regularly stepped interface boundary between h-BN (precipitate) and Si3N4 grains (within a silicon nitride particulate-reinforced silicon carbide composite) System: Si3N4-SiC composite, Composition: Not specified High resolution electron microscopy (HREM) 10 nm |
![]() |
Micrograph
552
:
An amorphous phase trapped at a triple junction between Si3N4 grains (within a silicon nitride particulate-reinforced silicon carbide composite). System: Si3N4-SiC composite, Composition: Not specified High resolution electron microscopy (HREM) 20 nm |
![]() |
Micrograph
553
:
Image of part of a crystalline triple junction between SiC grains (within a silicon nitride particulate-reinforced silicon carbide composite) System: Si3N4-SiC composite, Composition: Not specified High resolution electron microscopy (HREM) 6 nm |
![]() |
Micrograph
554
:
Silicon carbide System: SiC, Composition: Not specified Photography (no microscope) 10 mm |
| Showing 51 - 60 of 77 micrographs | Page 1 2 3 4 5 6 7 8 | Previous | Next |