Keyword
4 micrographs for keyword fibril, ordered by micrograph number.
![]() |
Micrograph
590
:
Remnants of crazes on a polycarbonate fracture surface System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 10 μm |
![]() |
Micrograph
591
:
Crazing near a fracture surface in polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 80 μm |
![]() |
Micrograph
592
:
The tip of a craze in polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
593
:
Ductile tearing near a fracture surface in polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 100 μm |