Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
7 micrographs for keyword polycarbonate (PC), ordered by micrograph number.
![]() |
Micrograph
559
:
Shear bands in stressed polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 800 μm |
![]() |
Micrograph
570
:
Strain-induced birefringence in a notched polycarbonate bar System: Polycarbonate (PC), Composition: Not specified Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
571
:
Strain-induced birefringence in a polycarbonate bar System: Polycarbonate (PC), Composition: Not specified Cross-polarised light microscopy 14 mm |
![]() |
Micrograph
590
:
Remnants of crazes on a polycarbonate fracture surface System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 10 μm |
![]() |
Micrograph
591
:
Crazing near a fracture surface in polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 80 μm |
![]() |
Micrograph
592
:
The tip of a craze in polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
593
:
Ductile tearing near a fracture surface in polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 100 μm |