Link to full record for micrograph 645 Micrograph 645 : An image of a single crystal alkane
System: Alkane, Composition: C294H590
Transmission electron microscopy (TEM)
2.4 μm
Link to full record for micrograph 649 Micrograph 649 : An image of an alkane crystal taken by AFM
System: Alkane, Composition: C36H74
Atomic force microscopy (AFM)
30 μm
Link to full record for micrograph 721 Micrograph 721 : Ni-Superalloy
System: Ni-X, Composition: Ni, Al, Re, W, Ta, Cr, Co, Ru (Ni-Superalloy)
Field emission gun scanning electron microscopy (FEGSEM) in secondary electron imaging (SEI) mode
10 μm
Link to full record for micrograph 722 Micrograph 722 : Ni-Superalloy
System: Ni-X, Composition: Ni, Al, Re, W, Ta, Cr, Co, Ru (Ni-Superalloy)
Field emission gun scanning electron microscopy (FEGSEM) in secondary electron imaging (SEI) mode
6 μm
Link to full record for micrograph 723 Micrograph 723 : Ni-Superalloy
System: Ni-X, Composition: Ni, Al, Re, W, Ta, Cr, Co, Ru (Ni-Superalloy)
Transmission electron microscopy (TEM)
200 nm