Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
9 micrographs for keyword heat treatment, ordered by micrograph number.
![]() |
Micrograph
657
:
Al-4 wt% Cu, age hardened alloy System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
658
:
Al-4 wt% Cu, over aged alloy System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
659
:
Al-4 wt% Cu, over aged alloy System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
660
:
Al-4 wt% Cu, over aged alloy System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
661
:
Al-4 wt% Cu, over aged alloy System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
662
:
Al-4 wt% Cu, over aged alloy System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
726
:
Ni-Superalloy, heat treated above gamma-prime solvus System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |
![]() |
Micrograph
780
:
Heat treated spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
781
:
Heat treated spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 50 μm |