535 micrographs for keyword metal, ordered by micrograph number.


Showing 161 - 170 of 535 micrographs Page 1 .. 14 15 16 17 18 19 20 .. 54 | Previous | Next

Link to full record for micrograph 265 Micrograph 265 : Fe, C 0.8 (wt%) steel, eutectoid transformation, spheroidised
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 266 Micrograph 266 : Fe, C 0.8 (wt%) steel, eutectoid transformation, spheroidised
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 267 Micrograph 267 : Fe, C 0.8 (wt%) steel, eutectoid transformation, spheroidised
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 268 Micrograph 268 : Fe, C 0.5 (wt%) steel, near a decarburised surface
System: Fe-C-X, Composition: Fe, C 0.5 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 269 Micrograph 269 : Fe, C 0.6 (wt%) steel, hard drawn
System: Fe-C-X, Composition: Fe, C 0.6 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 270 Micrograph 270 : Fe, C 0.6 (wt%) steel, hard drawn
System: Fe-C-X, Composition: Fe, C 0.6 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 271 Micrograph 271 : Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C
System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 272 Micrograph 272 : Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C
System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 273 Micrograph 273 : Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C
System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 274 Micrograph 274 : Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C
System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%)
Reflected light microscopy
400 μm

Showing 161 - 170 of 535 micrographs Page 1 .. 14 15 16 17 18 19 20 .. 54 | Previous | Next