535 micrographs for keyword metal, ordered by micrograph number.
| Showing 301 - 310 of 535 micrographs | Page 1 .. 28 29 30 31 32 33 34 .. 54 | Previous | Next |
![]() |
Micrograph
412
:
Cast iron, containing phosphorus System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
413
:
Cast iron, containing phosphorus System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
414
:
Cast iron, containing phosphorus System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
415
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 800 μm |
![]() |
Micrograph
416
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
![]() |
Micrograph
417
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy, polarised with wave-plate 800 μm |
![]() |
Micrograph
418
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
![]() |
Micrograph
419
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 100 μm |
![]() |
Micrograph
420
:
Commercial brass, ~30% Zn, displaying dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
421
:
Commercial brass, ~30% Zn, displaying dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%) Reflected light microscopy 400 μm |