Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
535 micrographs for keyword metal, ordered by micrograph number.
| Showing 421 - 430 of 535 micrographs | Page 1 .. 40 41 42 43 44 45 46 .. 54 | Previous | Next |
![]() |
Micrograph
605
:
Fracture surface formed by hot tearing (solidification cracking) System: Al, Composition: Commercial purity (99.5%) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
607
:
Fibre fracture in a metal matrix composite System: Al, Composition: Commercial purity (99.5%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
608
:
Channelling contrast TEM image of subgrains of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Transmission electron microscopy (TEM) 600 nm |
![]() |
Micrograph
609
:
The grain structure of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
613
:
Facetted aluminium dendrites System: Al-Sn, Composition: Al 15, Sn 85 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
614
:
Rapid solidification in an atomised droplet System: Al-Mg, Composition: Al 90, Mg 10 (wt%) Transmission electron microscopy (TEM) 500 nm |
![]() |
Micrograph
615
:
Cross-section of an aluminium casting System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy 10 mm |
![]() |
Micrograph
617
:
Deeply etched Co-dendrites System: Co-Sm-Cu, Composition: Co 70, Sm 10, Cu 20 (at%) Scanning electron microscopy (SEM) 80 μm |
![]() |
Micrograph
629
:
FORMGRIP closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |
![]() |
Micrograph
630
:
FOAMCARP closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |
| Showing 421 - 430 of 535 micrographs | Page 1 .. 40 41 42 43 44 45 46 .. 54 | Previous | Next |