Keyword
535 micrographs for keyword metal, ordered by micrograph number.
| Showing 501 - 510 of 535 micrographs | Page 1 .. 48 49 50 51 52 53 54 | Previous | Next |
![]() |
Micrograph
764
:
Bi 70, Sn 30 (wt%) System: Bi-Sn, Composition: Bi 70, Sn 30 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 10 μm |
![]() |
Micrograph
765
:
Bi 80, Sn 20 (wt%) System: Bi-Sn, Composition: Bi 80, Sn 20 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 300 μm |
![]() |
Micrograph
766
:
Bi 80, Sn 20 (wt%) System: Bi-Sn, Composition: Bi 80, Sn 20 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 100 μm |
![]() |
Micrograph
767
:
Bi 80, Sn 20 (wt%) System: Bi-Sn, Composition: Bi 80, Sn 20 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 10 μm |
![]() |
Micrograph
768
:
Bi 90, Sn 10 (wt%) System: Bi-Sn, Composition: Bi 90, Sn 10 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 300 μm |
![]() |
Micrograph
769
:
Bi 90, Sn 10 (wt%) System: Bi-Sn, Composition: Bi 90, Sn 10 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 100 μm |
![]() |
Micrograph
770
:
Bi 90, Sn 10 (wt%) System: Bi-Sn, Composition: Bi 90, Sn 10 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 10 μm |
![]() |
Micrograph
771
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Reflected light microscopy 100 μm |
![]() |
Micrograph
772
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 1 μm |
![]() |
Micrograph
773
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 1 μm |
| Showing 501 - 510 of 535 micrographs | Page 1 .. 48 49 50 51 52 53 54 | Previous | Next |