Micrograph no
769
Brief description
Bi 90, Sn 10 (wt%)
Keywords
alloy Link to MATTER Glossary entry for alloy, bismuth, metal, tin
Categories
Metal or alloy
System
Bi-Sn   Link to phase diagram
Composition
Bi 90, Sn 10 (wt%)
Standard codes
Reaction
Processing
Small casting in alumina crucible - air cooled.
Applications
Educational alloy - low melting point allows easy and safe use for students.
Sample preparation
Standard polishing techniques.
Technique
Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode
Length bar
100 μm
Further information
Some small scale ordering is apparent, with the pale areas almost pure bismuth, and the darker areas having near eutectic composition, and showing lamellae similar to those in micrograph 763.
Contributor
M Charles and A Cockburn
Organisation
Department of Materials Science and Metallurgy, University of Cambridge
Date
07/05/03
Licence for re-use
Attribution-Non-Commercial-Share Alike 2.0 UK: England & Wales