Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
30 micrographs for keyword stainless steel, ordered by micrograph number.
| Showing 11 - 20 of 30 micrographs | Page 1 2 3 | Previous | Next |
![]() |
Micrograph
803
:
Austenitic stainless steel solution treated, water quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Transmission electron microscopy (TEM) 1 μm |
![]() |
Micrograph
804
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Mo 2.5, C 0.25 (wt%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
805
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, V 5, C 0.1 (wt%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
806
:
Austenitic stainless steel water quenched then cooled, showing transformation to g in the a lamellae System: Fe-C-X, Composition: Fe, C 0.12, Mn 14.2, Cr 13.7 Reflected light microscopy 50 μm |
![]() |
Micrograph
809
:
Austenitic stainless steel solution treated, quenched, deformed in tension, then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Transmission electron microscopy (TEM) 1 μm |
![]() |
Micrograph
811
:
Austenitic stainless steel rapidly cooled, fracture surface of laboratory ingot System: Fe-C-X, Composition: Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
812
:
Austenitic stainless steel rapidly cooled, fracture surface of laboratory ingot System: Fe-C-X, Composition: Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
813
:
Austenitic stainless steel solution treated, quenched and tempered, with M23C6 precipitate System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Mo 1 (wt%) Transmission electron microscopy (TEM) 400 nm |
![]() |
Micrograph
814
:
Austenitic stainless steel solution treated, quenched and tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Transmission electron microscopy (TEM) 1 μm |
![]() |
Micrograph
816
:
Austenitic stainless steel solution treated, quenched and tempered, showing M23C6 precipitate System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Mo 1 (wt%) Transmission electron microscopy (TEM) 400 nm |
| Showing 11 - 20 of 30 micrographs | Page 1 2 3 | Previous | Next |