Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
65 micrographs for keyword aluminium, ordered by micrograph number.
| Showing 21 - 30 of 65 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
![]() |
Micrograph
140
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
141
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
142
:
Tough pitch copper, failed by fibrous ductile fracture. System: Cu, Composition: Tough pitch copper Scanning electron microscopy (SEM) 20 μm |
![]() |
Micrograph
148
:
Magnesia-chrome refractory brick System: MgO-Cr2O3, Composition: MgO 70, Cr2O3 19, Al2O3 4, Fe2O3 4, CaO 1, SiO2 1 (wt%) Reflected light microscopy 1 mm |
![]() |
Micrograph
149
:
Magnesia-chrome refractory brick System: MgO-Cr2O3, Composition: MgO 70, Cr2O3 19, Al2O3 4, Fe2O3 4, CaO 1, SiO2 1 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
150
:
Alumina-zirconia-silica (AZS) refractory brick System: Al2O3-ZrO2-SiO2, Composition: Al2O3 50, ZrO2 32, SiO2 15 (wt%), + trace alkalis Reflected light microscopy 300 μm |
![]() |
Micrograph
151
:
Alumina-graphite brick System: Al2O3-C-Si, Composition: Al2O3, C up to 30 (wt%), Si few% Reflected light microscopy 400 μm |
![]() |
Micrograph
154
:
Macor(TM) Machinable Glass Ceramic System: MAS (MgO-Al2O3-SiO2), Composition: SiO2 47, B2O3 8, Al2O3 17, MgO 14, K2O 9, F 6 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
156
:
Roll-bonded aluminium alloy diffusion couple annealed for 30 minutes at 600ºC. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 400 μm |
![]() |
Micrograph
157
:
Roll-bonded aluminium alloy diffusion couple annealed for 60 minutes at 600ºC. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 750 μm |
| Showing 21 - 30 of 65 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |