Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
65 micrographs for keyword aluminium, ordered by micrograph number.
| Showing 31 - 40 of 65 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
![]() |
Micrograph
158
:
Roll-bonded aluminium alloy diffusion couple in the as-rolled condition. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 400 μm |
![]() |
Micrograph
159
:
Roll-bonded aluminium alloy diffusion couple in the as-rolled condition. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 2 mm |
![]() |
Micrograph
604
:
Extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
608
:
Channelling contrast TEM image of subgrains of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Transmission electron microscopy (TEM) 600 nm |
![]() |
Micrograph
609
:
The grain structure of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
613
:
Facetted aluminium dendrites System: Al-Sn, Composition: Al 15, Sn 85 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
615
:
Cross-section of an aluminium casting System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy 10 mm |
![]() |
Micrograph
629
:
FORMGRIP closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |
![]() |
Micrograph
630
:
FOAMCARP closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |
![]() |
Micrograph
631
:
Coarse open celled aluminium foam produced by infiltration of sintered salt (FOAM-U-LIKE) System: Al, Composition: Not specified Photography (no microscope) 6 mm |
| Showing 31 - 40 of 65 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |