Keyword
65 micrographs for keyword aluminium, ordered by micrograph number.
| Showing 41 - 50 of 65 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
![]() |
Micrograph
632
:
Open-celled aluminium foam System: Al, Composition: Not specified Photography (no microscope) 8 mm |
![]() |
Micrograph
633
:
Cross-section of an aluminium foam slab produced by gas injection System: Al, Composition: Not specified Photography (no microscope) 10 mm |
![]() |
Micrograph
634
:
Solid-gas eutectic solidification (Gasar) aluminium foam System: Al, Composition: Not specified Photography (no microscope) 120 μm |
![]() |
Micrograph
635
:
Open celled aluminium foam produced by infiltration of sintered salt System: Al, Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
![]() |
Micrograph
636
:
Alporas' closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |
![]() |
Micrograph
656
:
Al, commercial purity System: Al, Composition: Not specified Reflected light microscopy 10 mm |
![]() |
Micrograph
657
:
Al-4 wt% Cu, age hardened alloy System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
658
:
Al-4 wt% Cu, over aged alloy System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
659
:
Al-4 wt% Cu, over aged alloy System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
660
:
Al-4 wt% Cu, over aged alloy System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 100 μm |