272 micrographs for keyword iron, ordered by micrograph number.


Showing 31 - 40 of 272 micrographs Page 1 2 3 4 5 6 7 .. 28 | Previous | Next

Link to full record for micrograph 73 Micrograph 73 : Ni-hard iron
System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron)
Reflected light microscopy
80 μm
Link to full record for micrograph 78 Micrograph 78 : Forging steel, brittle, intergranular fracture
System: Fe-C-X, Composition: Forging steel
Scanning electron microscopy (SEM)
800 μm
Link to full record for micrograph 134 Micrograph 134 : High carbon steel
System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%)
Transmission electron microscopy (TEM)
600 nm
Link to full record for micrograph 135 Micrograph 135 : High carbon steel
System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%)
Transmission electron microscopy (TEM)
1.5 μm
Link to full record for micrograph 148 Micrograph 148 : Magnesia-chrome refractory brick
System: MgO-Cr2O3, Composition: MgO 70, Cr2O3 19, Al2O3 4, Fe2O3 4, CaO 1, SiO2 1 (wt%)
Reflected light microscopy
1 mm
Link to full record for micrograph 149 Micrograph 149 : Magnesia-chrome refractory brick
System: MgO-Cr2O3, Composition: MgO 70, Cr2O3 19, Al2O3 4, Fe2O3 4, CaO 1, SiO2 1 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 152 Micrograph 152 : Barium Hexaferrite
System: BaO-Fe2O3, Composition: BaO . 6Fe2O3
Reflected light microscopy
100 μm
Link to full record for micrograph 201 Micrograph 201 : Normalised low carbon steel, showing directionality
System: Fe-C-X, Composition: Wrought iron (plain carbon steel)
Reflected light microscopy
400 μm
Link to full record for micrograph 202 Micrograph 202 : Normalised low carbon steel, showing directionality
System: Fe-C-X, Composition: Wrought iron (plain carbon steel)
Reflected light microscopy
200 μm
Link to full record for micrograph 203 Micrograph 203 : Normalised low carbon manganese steel, showing directionality
System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%)
Reflected light microscopy
400 μm