Keyword
172 micrographs for keyword steel, ordered by micrograph number.
Showing 21 - 30 of 172 micrographs | Page 1 2 3 4 5 6 7 .. 18 | Previous | Next |
![]() |
Micrograph
135
:
High carbon steel System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%) Transmission electron microscopy (TEM) 1.5 μm |
![]() |
Micrograph
143
:
Notched low carbon ferritic steel, failed through cleavage. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 20 μm |
![]() |
Micrograph
146
:
HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
147
:
HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
201
:
Normalised low carbon steel, showing directionality System: Fe-C-X, Composition: Wrought iron (plain carbon steel) Reflected light microscopy 400 μm |
![]() |
Micrograph
202
:
Normalised low carbon steel, showing directionality System: Fe-C-X, Composition: Wrought iron (plain carbon steel) Reflected light microscopy 200 μm |
![]() |
Micrograph
203
:
Normalised low carbon manganese steel, showing directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
204
:
Normalised low carbon manganese steel, showing directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
205
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
206
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 200 μm |
Showing 21 - 30 of 172 micrographs | Page 1 2 3 4 5 6 7 .. 18 | Previous | Next |