Link to full record for micrograph 530 Micrograph 530 : Cu - 20% Sn bronze, cast annealed
System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 531 Micrograph 531 : Cu - 20% Sn bronze, cast annealed
System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 532 Micrograph 532 : Cu - 20% Sn bronze, cast annealed
System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 533 Micrograph 533 : Cu - 20% Sn bronze, cast annealed
System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 534 Micrograph 534 : Cu - Sn, cast annealed
System: Cu-Sn, Composition: Not specified
Reflected light microscopy
800 μm
Link to full record for micrograph 535 Micrograph 535 : Cu - Sn, cast annealed
System: Cu-Sn, Composition: Not specified
Reflected light microscopy
400 μm
Link to full record for micrograph 536 Micrograph 536 : Cu - Sn, cast annealed
System: Cu-Sn, Composition: Not specified
Reflected light microscopy
200 μm
Link to full record for micrograph 537 Micrograph 537 : Cu - Sn, cast annealed
System: Cu-Sn, Composition: Not specified
Reflected light microscopy
100 μm
Link to full record for micrograph 613 Micrograph 613 : Facetted aluminium dendrites
System: Al-Sn, Composition: Al 15, Sn 85 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 744 Micrograph 744 : Bi 10, Sn 90 (wt%)
System: Bi-Sn, Composition: Bi 10, Sn 90 (wt%)
Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode
300 μm