86 micrographs for keyword tin, ordered by micrograph number.


Showing 81 - 86 of 86 micrographs Page 1 .. 3 4 5 6 7 8 9 | Previous | Next

Link to full record for micrograph 765 Micrograph 765 : Bi 80, Sn 20 (wt%)
System: Bi-Sn, Composition: Bi 80, Sn 20 (wt%)
Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode
300 μm
Link to full record for micrograph 766 Micrograph 766 : Bi 80, Sn 20 (wt%)
System: Bi-Sn, Composition: Bi 80, Sn 20 (wt%)
Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode
100 μm
Link to full record for micrograph 767 Micrograph 767 : Bi 80, Sn 20 (wt%)
System: Bi-Sn, Composition: Bi 80, Sn 20 (wt%)
Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode
10 μm
Link to full record for micrograph 768 Micrograph 768 : Bi 90, Sn 10 (wt%)
System: Bi-Sn, Composition: Bi 90, Sn 10 (wt%)
Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode
300 μm
Link to full record for micrograph 769 Micrograph 769 : Bi 90, Sn 10 (wt%)
System: Bi-Sn, Composition: Bi 90, Sn 10 (wt%)
Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode
100 μm
Link to full record for micrograph 770 Micrograph 770 : Bi 90, Sn 10 (wt%)
System: Bi-Sn, Composition: Bi 90, Sn 10 (wt%)
Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode
10 μm