Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
80 micrographs for keyword zinc, ordered by micrograph number.
| Showing 1 - 10 of 80 micrographs | Page 1 2 3 4 5 6 7 8 | Previous | Next |
![]() |
Micrograph
29
:
Cu 70, Zn 30 (wt%), annealed and cold rolled System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
30
:
Cu 70, Zn 30 (wt%), annealed and cold rolled System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
31
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
32
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
33
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
34
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
35
:
Cu 70, Zn 30 (wt%), faster recrystallisation - finer grain size System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
36
:
Cu 60, Zn 40 (wt%), quenched - metastable b grains System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
37
:
Cu 70, Zn 30 (wt%), slow cooling - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
41
:
Zn, cold rolled - mechanical twins System: Zn, Composition: Not specified Reflected light microscopy 400 μm |
| Showing 1 - 10 of 80 micrographs | Page 1 2 3 4 5 6 7 8 | Previous | Next |