4 micrographs for keyword titanium, ordered by micrograph number.
![]() |
Micrograph
54
:
Ti, Al 6, V 4 (wt%), Widmanstätten microstructure System: Ti-Al-V, Composition: Ti, Al 6, V 4 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
55
:
Ti, Al 6, V 4 (wt%), Widmanstätten microstructure System: Ti-Al-V, Composition: Ti, Al 6, V 4 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
136
:
Nd4SrTi5O17 Oxide sample viewed along the [100] direction. System: Nd-Sr-Ti, Composition: Nd4SrTi5O17 High resolution electron microscopy (HREM) 4 nm |
![]() |
Micrograph
153
:
Barium Titanate Ag/Pd Multilayer Capacitor System: BaTiO3 Ag/Pd, Composition: BaTiO3 Reflected light microscopy 300 μm |