Micrograph 159 and full record
- Micrograph no
- 159
- Brief description
- Roll-bonded aluminium alloy diffusion couple in the as-rolled condition.
- Keywords
- alloy
, aluminium
, diffusion couple
, metal, roll-bonding 
- Categories
- Metal or alloy
- System
- Al-Fe-Mn/Al-Si
- Composition
- Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%)
- Standard codes
- Reaction
- Processing
- Mechanical roll-bonding; reduction in thickness of about 90%.
- Applications
- The couple was made to investigate diffusion of silicon through the Al-0.5Fe-1.0Mn (wt.%) alloy during annealing.
- Sample preparation
- Electrolytically etched using Barker's reagent.
- Technique
- Cross-polarised light microscopy
- Length bar
- 2 mm
- Further information
- This micrograph shows the grain structure of a roll-bonded aluminium alloy diffusion couple in the as-rolled condition. The upper half of the couple is Al-0.5Fe-1.0Mn (wt.%), the lower half is Al-1.0Si (wt.%). Rolling heavily deforms the microstructure, producing thin, elongated grains parallel to the roll-bonded interface.
The Barker's etch produces a thick oxide layer on the grains of aluminium (anodising). When viewed in cross-polarised light, interference in the oxide layer produces colours which depend on grain orientation, hence the grain structure is imaged. Prior to roll-bonding the Al-Si alloy was solution-treated, creating recrystallized grains that were much larger than the cellular microstructure of the Al-Fe-Mn alloy. This difference in scale of microstructure can be seen in the rolled diffusion couple. - Contributor
- D T L Alexander
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 21/05/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs
- Micrograph 156: Roll-bonded aluminium alloy diffusion couple annealed for 30 minutes at 600ºC. (400 μm)
- Micrograph 157: Roll-bonded aluminium alloy diffusion couple annealed for 60 minutes at 600ºC. (750 μm)
- Micrograph 158: Roll-bonded aluminium alloy diffusion couple in the as-rolled condition. (400 μm)
View image alone .. in a new window
Help is available on downloading images