Micrograph 208 and full record
- Micrograph no
- 208
- Brief description
- Normalised low carbon manganese steel, taken transverse to directionality
- Keywords
- alloy
, carbon, eutectoid reaction
, iron, metal, pearlite
, steel 
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C 0.2 (wt%)
- Standard codes
- Reaction
- Processing
- Hot worked normalised 1000 ºC
- Applications
- Sample preparation
- Nital
- Technique
- Reflected light microscopy
- Length bar
- 400 μm
- Further information
- Low carbon steel with a microstructure consisting mostly of ferrite with the darker pearlite surrounding the lighter ferrite. This sample has been normalised, recrystallising the ferrite. The pearlite is unable to do this and consequently retains its directionality.
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02