Micrograph 459 and full record
- Micrograph no
- 459
- Brief description
- Brass, exhibiting grain boundary nucleation
- Keywords
- alloy
, brass
, copper, metal, zinc - Categories
- Metal or alloy
- System
- Cu-Zn
- Composition
- Cu 50, Zn 50 (wt%)
- Standard codes
- Reaction
- Processing
- Cast
- Applications
- Sample preparation
- Ammonium persulphate
- Technique
- Reflected light microscopy
- Length bar
- 400 μm
- Further information
- A high zinc brass that forms large grains of b phase (yellow areas, due to higher copper content) and subsequently grains of g form on b grain boundaries and also on non-metallic inclusions in the alloy.
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs