Micrograph 491 and full record
- Micrograph no
- 491
- Brief description
- Cu 70, Sn 30 (wt%) bronze, as cast
- Keywords
- alloy
, bronze
, copper, metal, tin - Categories
- Metal or alloy
- System
- Cu-Sn
- Composition
- Cu 70, Sn 30 (wt%)
- Standard codes
- Reaction
- Processing
- Cast
- Applications
- Sample preparation
- Ferric chloride
- Technique
- Reflected light microscopy
- Length bar
- 400 μm
- Further information
- High tin Cu-Sn alloy. The phase diagram of this system is complicated, at room temperature the equilibrium phases are a (copper) and e.
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs