Micrograph no
707
Brief description
Cu-? wt% P
Keywords
alloy Link to MATTER Glossary entry for alloy, copper, dendrite Link to MATTER Glossary entry for dendrite, metal, phosphorus Link to MATTER Glossary entry for phosphorus
Categories
Metal or alloy
System
Cu-P   Link to phase diagram
Composition
Not specified
Standard codes
Reaction
Processing
Applications
Sample preparation
Technique
Reflected light microscopy
Length bar
100 μm
Further information
Contributor
Dr J Marrow
Organisation
Department of Materials Science, University of Manchester and UMIST
Date
07/11/02
Licence for re-use
Attribution-Non-Commercial-Share Alike 2.0 UK: England & Wales
Related micrographs

View image alone .. in a new window

View micrograph only

View full record only

Help is available on downloading images