Micrograph 772 and full record
- Micrograph no
- 772
- Brief description
- Austenitic stainless steel
- Keywords
- alloy , annealing twins , austenite , dislocation , grain , metal, recrystallisation , stainless steel, steel
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Stainless steel
- Standard codes
- Reaction
- Processing
- The sample was cold-deformed by rolling and then annealed at 704°C for one hour.
- Applications
- Sample preparation
- Technique
- Transmission electron microscopy (TEM)
- Length bar
- 1 μm
- Further information
- This is a transmission electron micrograph taken at 200 kV, from a thin foil sample of "302AA" austenitic stainless steel. The sample was cold-deformed by rolling and then annealed at 704°C for one hour. The image shows a recrystallised grain which is relatively free of dislocations, surrounded by a deformed matrix which has a high dislocation density. The recrystallised grain contains annealing twins (parallel bands with different contrast).
Source: http://www.msm.cam.ac.uk/phase-trans/abstracts/annealing.twin.html. - Contributor
- Prof H K D H Bhadeshia
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 18/07/03
- Licence for re-use
- Attribution-NonCommercial-ShareAlike 4.0 International
- Related micrographs
View image alone .. in a new window
Help is available on downloading images