Micrograph 869 and full record
- Micrograph no
- 869
- Brief description
- Diamond
- Keywords
- Categories
- Ceramic
- System
- C
- Composition
- Carbon
- Standard codes
- Reaction
- Processing
- Applications
- Sample preparation
- Technique
- Atomic force microscopy (AFM)
- Length bar
- 20 μm
- Further information
- A diamond nano-indentation tip, made by hand using jeweler's lapping techniques.
- Contributor
- Jeff Wheeler
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 12/08/10
- Licence for re-use