Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

DoITPoMS Micrograph Library Micrograph 898 and full record

Micrograph 898 and full record

Link to image file for micrograph 898
Micrograph no
898
Brief description
Dasht-e-Kavir, Saghand - Posht-e-Badam. Copper slag
Keywords
Categories
Metal or alloy
System
Cu production
Composition
Not specified
Standard codes
Reaction
Processing
Applications
Sample preparation
polished surface
Technique
Reflected light microscopy
Length bar
100 μm
Further information
Contributor
Dr Ingo Keesmann
Organisation
Johannes Gutenberg-Universitat Mainz
Date
15/10/10
Licence for re-use
DoITPoMS standard terms of use

View image alone .. in a new window

View micrograph only

View full record only

Help is available on downloading images