System
333 micrographs for system Fe-C-X, ordered by micrograph number.
Showing 281 - 290 of 333 micrographs | Page 1 .. 26 27 28 29 30 31 32 .. 34 | Previous | Next |
Micrograph
795
:
Blackheart cast iron System: Fe-C-X, Composition: Blackheart cast iron Reflected light microscopy 100 μm |
|
Micrograph
796
:
Blackheart cast iron System: Fe-C-X, Composition: Blackheart cast iron Reflected light microscopy 100 μm |
|
Micrograph
797
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
798
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 20 μm |
|
Micrograph
799
:
Austenitic stainless steel solution treated, water quenched and tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Scanning electron microscopy (SEM) 2 μm |
|
Micrograph
800
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Nb 1 (wt%) Scanning electron microscopy (SEM) 1 μm |
|
Micrograph
801
:
Austenitic stainless steel solution treated, water quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Transmission electron microscopy (TEM) 400 nm |
|
Micrograph
802
:
Austenitic stainless steel solution treated, water quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
803
:
Austenitic stainless steel solution treated, water quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
804
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Mo 2.5, C 0.25 (wt%) Scanning electron microscopy (SEM) 4 μm |
Showing 281 - 290 of 333 micrographs | Page 1 .. 26 27 28 29 30 31 32 .. 34 | Previous | Next |