333 micrographs for system Fe-C-X, ordered by micrograph number.
Showing 331 - 333 of 333 micrographs | Page 1 .. 28 29 30 31 32 33 34 | Previous | Next |
Micrograph
871
:
Low Carbon Steel System: Fe-C-X, Composition: Fe, C 0.9 (wt%) Atomic force microscopy (AFM) 30 μm |
|
Micrograph
935
:
Dasht-e-Kavir, Saghand - Posht-e-Badam. Copper slag System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Reflected light microscopy 2 mm |
|
Micrograph
936
:
Shirnu Central Iran. Copper production slag System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Transmitted light microscopy 1 mm |